High Temperature Microstructural Stability of Si3N4 in TiAl Alloys

Alloys of Ti-50 at.% Al with (3 and 10)wt.% Si3N4 particles were prepared by a mechanical alloying-spark plasma sintering (MA-SPS) method. The matrix consisted primarily of TiAl, Ti2AlN, TiN. Si3N4 was unstable in the matrix and started to decompose forming a Ti5Si3 reaction layer on the surface of...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Materials science forum 2007-01, Vol.534-536, p.1577-1580
Hauptverfasser: Lee, Dong Bok, Choi, Jee Hoon
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Alloys of Ti-50 at.% Al with (3 and 10)wt.% Si3N4 particles were prepared by a mechanical alloying-spark plasma sintering (MA-SPS) method. The matrix consisted primarily of TiAl, Ti2AlN, TiN. Si3N4 was unstable in the matrix and started to decompose forming a Ti5Si3 reaction layer on the surface of former Si3N4 particles during sintering and heat treatment at 1373 K.
ISSN:0255-5476
1662-9752
1662-9752