The effect of the atmosphere and the role of pore filling on the sintering of aluminium

Alloys of Al–3.8Cu–1Mg–0.7Si, Al–4Cu–0.6Si–0.1Mg, Al–4Cu–1.2Mg and Al–1.9Mg–1.9Si were made using air atomised powder and conventional press-and-sinter powder metallurgy techniques. These were sintered under nitrogen with a controlled water content which varied from 3 to 630 ppm (a dew point of −69...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Acta materialia 2006-01, Vol.54 (1), p.131-138
Hauptverfasser: Schaffer, G.B., Hall, B.J., Bonner, S.J., Huo, S.H., Sercombe, T.B.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Alloys of Al–3.8Cu–1Mg–0.7Si, Al–4Cu–0.6Si–0.1Mg, Al–4Cu–1.2Mg and Al–1.9Mg–1.9Si were made using air atomised powder and conventional press-and-sinter powder metallurgy techniques. These were sintered under nitrogen with a controlled water content which varied from 3 to 630 ppm (a dew point of −69 to −25 °C), nitrogen–5%hydrogen, argon and argon–5%hydrogen, all at atmospheric pressure, or a vacuum of