Thermal treatment on composite γ-zirconium phosphate-silica

The prepared amorphous gamma-ZrP\SiO2 composite had a complicated composition, since a part of gamma-ZrP is converted to alpha-form during the exfoliation of it. The gamma-ZrP\SiO2 composite have specific surface area of 421 mg. The acidic P-OH groups of the lamellae species placed on the surface (i...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of thermal analysis and calorimetry 2006-08, Vol.85 (2), p.329-333
Hauptverfasser: SZIRTES, L, MEGYERI, J, KUZMANN, E
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The prepared amorphous gamma-ZrP\SiO2 composite had a complicated composition, since a part of gamma-ZrP is converted to alpha-form during the exfoliation of it. The gamma-ZrP\SiO2 composite have specific surface area of 421 mg. The acidic P-OH groups of the lamellae species placed on the surface (it is {approximately equal to}1.0 meq g), do not destroy until the temperature of 1030 K. During the thermal treatment the total mass loss of 7.79% was found. This value corresponds to 0.42 mole of H2O per molecule unit. The water loss process was found very slow, because of the placing of bilamellar species in the composite.