Electrical and thermal transport properties of Ba6C60 compound

Bulk Ba6C60 fulleride has been prepared by solid-state reaction and spark plasma sintering (SPS) technique. We report measurements of electrical resistivity, Seebeck coefficient, thermal conductivity and Hall effect. The compound is metallic with high electron concentration and low mobility. The val...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Physica. B, Condensed matter Condensed matter, 2005-12, Vol.369 (1-4), p.28-32
Hauptverfasser: SHI, X, CHEN, L. D, BAI, S. Q, ZHANG, W. B, ZHAO, X. Y
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Bulk Ba6C60 fulleride has been prepared by solid-state reaction and spark plasma sintering (SPS) technique. We report measurements of electrical resistivity, Seebeck coefficient, thermal conductivity and Hall effect. The compound is metallic with high electron concentration and low mobility. The values of electrical resistivity and thermopower are also low, consistent with the Hall data. The lattice thermal conductivity for Ba6C60 fulleride at room temperature is estimated to be about 1.44W/mK, close to the value of amorphous SiO2. This low value of lattice thermal conductivity is ascribed to strong resonance scatterings by C60 cluster vibrations.
ISSN:0921-4526
1873-2135
DOI:10.1016/j.physb.2005.07.023