Alumina fine powder (0.6 μm) is granulated by 3 mass% PVA. The granule admixed with liquid paraffin are formed by a single-action tooling to columnar-shaped green compact, diameter: 60 mm, height: 60 mm and mass: 450 g. Green density increases according to the content of liquid paraffin. Debinding o...
Gespeichert in:
Veröffentlicht in: | Journal of the Japan Society of Powder and Powder Metallurgy 2005, Vol.52(5), pp.334-338 |
---|---|
Hauptverfasser: | , , , |
Format: | Artikel |
Sprache: | jpn |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Alumina fine powder (0.6 μm) is granulated by 3 mass% PVA. The granule admixed with liquid paraffin are formed by a single-action tooling to columnar-shaped green compact, diameter: 60 mm, height: 60 mm and mass: 450 g. Green density increases according to the content of liquid paraffin. Debinding of green compact admixed with a lot of liquid paraffin is succeeded without cracking on compact by thermal debinding technique after extracting liquid paraffin in an organic solvent to pre-baked compact. Sintered density and dimensional precision of sintered compact formed by flow compaction are improved by liquid paraffin content of 7.5 mass% and by compacting pressure of 98 MPa. |
---|---|