Phosphorus recovery from phosphate tailings through a two-stage leaching-precipitation process: Toward the harmless and reduction treatment of P-bearing wastes

To achieve highly efficient extraction of phosphorus (P) and comprehensive utilization of phosphate tailings, a two-stage leaching-precipitation method was proposed. Phosphate tailings primarily consisted of dolomite, fluorapatite, and quartz. During the first-stage leaching, the large majority of d...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Environmental research 2024-05, Vol.248, p.118328-118328, Article 118328
Hauptverfasser: Yu, Yao-hui, Du, Chuan-ming, Zhang, Yu-tang, Yuan, Rui-yuan
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:To achieve highly efficient extraction of phosphorus (P) and comprehensive utilization of phosphate tailings, a two-stage leaching-precipitation method was proposed. Phosphate tailings primarily consisted of dolomite, fluorapatite, and quartz. During the first-stage leaching, the large majority of dolomite was selectively dissolved and the leaching efficiency of Mg reached 93.1 % at pH 2.0 and 60 °C. The subsequent second-stage leaching of fluorapatite was performed and the P leaching efficiency was 98.8 % at pH 1.5 and 20 °C, while the quartz remained in the residue. Through two-stage leaching, a stepwise leaching of dolomite and fluorapatite was achieved. After chemical precipitation, calcium phosphate with a high purity of 97.9 % was obtained; and the total recovery efficiency of P exceeded 98 %. The obtained calcium phosphate can be a raw material in the phosphorus chemical industry, while the Mg-rich leachate and the final quartz-rich residue have the potential for Mg extraction and the production of mortars or geopolymers, respectively. The two-stage leaching-precipitation process could significantly reduce the leaching costs, and enhance the reaction rates. It is expected to realize a volume reduction and efficient resource utilization of the phosphate tailings by using this sustainable and promising solution. •A new method of P extraction and utilization of phosphate tailings was proposed.•A stepwise dissolution of dolomite and fluorapatite was achieved.•High-grade calcium phosphates were recovered from the phosphate tailings.•CaHPO4 and Ca10(PO4)6(OH)2 were obtained at pH 6.0 and 8.0, respectively.
ISSN:0013-9351
1096-0953
DOI:10.1016/j.envres.2024.118328