Study of the coercivity for Nd-Fe-B-Ga sintered magnets
The Ga-composition dependence of the Curie temperature, the anisotropy field, and the coercivity are studied for Nd-Fe-B-Ga sintered magnets. It is shown that a smaller addition of Ga atoms increases not only the Curie temperature but also the coercivity. A rise in coercivity does not result from th...
Gespeichert in:
Veröffentlicht in: | IEEE (Institute of Electrical and Electronics Engineers) Transactions on Magnetics; (USA) 1989-09, Vol.25 (5), p.3429-3430 |
---|---|
Hauptverfasser: | , , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The Ga-composition dependence of the Curie temperature, the anisotropy field, and the coercivity are studied for Nd-Fe-B-Ga sintered magnets. It is shown that a smaller addition of Ga atoms increases not only the Curie temperature but also the coercivity. A rise in coercivity does not result from the change of anisotropy field for Nd/sub 16/Fe/sub 77/B/sub 7-x/Ga/sub x/ sintered magnets. It is also found that the coercivity for a Nd/sub 16/Fe/sub 77/Ga/sub 2/B/sub 5/ magnet, which has lower B content, is controlled by nucleation whereas for the magnet Nd/sub 13.5/Dy/sub 1.5/Fe/sub 75/Al/sub 2/B/sub 8/ (iH/sub c/=18 kOe), two kinds of coercivity mechanisms (pinning and nucleation) coexist.< > |
---|---|
ISSN: | 0018-9464 1941-0069 |
DOI: | 10.1109/20.42324 |