Synthesis and characterisation of organosoluble polyimides containing the anisyl moiety
A new type of diamine monomer containing the anisyl moiety was synthesized via a straight‐forward one‐step procedure. Anisaldehyde was reacted with 2,6‐dimethylaniline in the presence of dry HCl to attain bis(4‐amino‐3,5‐dimethylphenyl)anisylmethane. A series of organo‐soluble polyimides were prepar...
Gespeichert in:
Veröffentlicht in: | Polymer international 2004-10, Vol.53 (10), p.1442-1447 |
---|---|
Hauptverfasser: | , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A new type of diamine monomer containing the anisyl moiety was synthesized via a straight‐forward one‐step procedure. Anisaldehyde was reacted with 2,6‐dimethylaniline in the presence of dry HCl to attain bis(4‐amino‐3,5‐dimethylphenyl)anisylmethane. A series of organo‐soluble polyimides were prepared using the anisyl diamine and various aromatic dianhydrides via a two step method involving thermal imidization. All polyimides are soluble in strong polar solvents such as N‐methyl‐2‐pyrollidone, N,N‐Dimethylformamide, and N,N‐DimethylAcetamide. The polyimides show excellent thermal stability and good mechanical properties. The glass transition temperatures of the polyimides are in the range 265–294 °C. The tensile strengths are in the range 79–99 MPa and the temperatures at which 10 % weight loss occurs are in the range 460–496 °C. Copyright © 2004 Society of Chemical Industry |
---|---|
ISSN: | 0959-8103 1097-0126 |
DOI: | 10.1002/pi.1551 |