Leaching of a sphalerite concentrate with H2SO4-HNO3 solutions in the presence of C2Cl4
The enhanced leaching of sphalerite concentrates in H2SO4-HNO3 solutions and the extraction of sulfur with tetrachloroethylene were studied. Variables of the process were investigated including leaching temperature, reaction time, liquid/solid ratio, and tetrachloroethylene concentration. The number...
Gespeichert in:
Veröffentlicht in: | Hydrometallurgy 2005-12, Vol.80 (4), p.265-271 |
---|---|
Hauptverfasser: | , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The enhanced leaching of sphalerite concentrates in H2SO4-HNO3 solutions and the extraction of sulfur with tetrachloroethylene were studied. Variables of the process were investigated including leaching temperature, reaction time, liquid/solid ratio, and tetrachloroethylene concentration. The number of cycles that tetrachloroethylene could be recycled did not have a significant effect on zinc extraction. The results indicated that 99.6% zinc extraction was obtained after three hours of leaching at 85 DGC and 0.1 MPa O2, when 20 g of sphalerite concentrate were leached in a 200 ml solution containing 2.0 mol/L H2SO4 and 0.2 mol/L HNO3, in the presence of 10 ml C2Cl4. Leaching rates were significantly improved under these conditions. |
---|---|
ISSN: | 0304-386X 1879-1158 |
DOI: | 10.1016/j.hydromet.2005.08.004 |