High-temperature tribological properties of Al2O3, Ni-20 mass% Cr and NiAl spark-plasma-sintered composites containing BaF2-CaF2 phase

A;2O3, Ni-20 mass% Cr, NiAl-based composites containing BaF2, CaF2 and SrF2 as solid lubricants were prepared by spark plasma sintering, and their microstructure and high-temperature friction and wear properties were examined. Al2O3-31BaF2-19CaF2 (mass%) composites prepared by spark plasma sintering...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Wear 2005-07, Vol.259 (1), p.626-633
Hauptverfasser: MURAKAMI, T, OUYANG, J. H, SASAKI, S, UMEDA, K, YONEYAMA, Y
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A;2O3, Ni-20 mass% Cr, NiAl-based composites containing BaF2, CaF2 and SrF2 as solid lubricants were prepared by spark plasma sintering, and their microstructure and high-temperature friction and wear properties were examined. Al2O3-31BaF2-19CaF2 (mass%) composites prepared by spark plasma sintering at 1273 K contained a fine lamellar structure, which consisted of BaF2 and CaF2 phases. The Al2O3-31 BaF2-19CaF2 (mass%) composites showed a low friction coefficient (0.3-0.4) at temperatures between room temperature and 1073 K, in addition that they showed the lowest wear rate at 873 K. In this study, a tentative BaF2-CaF2-SrF2 ternary phase diagram was also constructed, which clarified that the BaF2-CaF2-SrF2 ternary system has a large solid solution region at 1473 K.