Low temperature synthesis of boron phosphide nanocrystals
Nanocrystalline boron phosphide (BP) was successfully synthesized at low temperature (400 °C) by a simple reaction between PCl 3 and NaBF 4 using Na as reductant. X-ray powder diffraction patterns indicated that the resultant was cubic BP with a lattice constant a=4.533 Å. Transmission electron micr...
Gespeichert in:
Veröffentlicht in: | Materials letters 2005-04, Vol.59 (8), p.865-867 |
---|---|
Hauptverfasser: | , , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Nanocrystalline boron phosphide (BP) was successfully synthesized at low temperature (400 °C) by a simple reaction between PCl
3 and NaBF
4 using Na as reductant. X-ray powder diffraction patterns indicated that the resultant was cubic BP with a lattice constant
a=4.533 Å. Transmission electron microscopy revealed that the crystals were composed of spherical particles with the diameter of 80 nm or so and lots of worm-like rods. The possible formation mechanism was also investigated. |
---|---|