Vacancy-Like Defects in Doped Pb(Zr60Ti40)O3 Observed by Positron Lifetime and Coincident Doppler Spectroscopy

Ferroelectric Pb(Zr60Ti40)O3 ceramics sintered for 6 hours at 1050DGC in air and doped with La or Nb in the range 0.5 to 6 mol% have been investigated by positron lifetime spectroscopy and two-dimensional coincident Doppler measurements. The undoped samples show two lifetime components with a defect...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Materials science forum 2004-01, Vol.445-446, p.171-173
Hauptverfasser: Hoffmann, Michael J., Kungl, Hans, Gottschalk, Sebastian, Puff, Werner, Balogh, Adam G.
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Ferroelectric Pb(Zr60Ti40)O3 ceramics sintered for 6 hours at 1050DGC in air and doped with La or Nb in the range 0.5 to 6 mol% have been investigated by positron lifetime spectroscopy and two-dimensional coincident Doppler measurements. The undoped samples show two lifetime components with a defect lifetime of about 250 ps. After doping this defect lifetime increases to about 295 ps. The influence of the doping on the Doppler spectra is extremely small. Additional XRD pattern show a significant correlation between doping and lattice structure.