Surface morphological properties of sol-gel derived SiO2 fiber

In this study, sol-gel derived SiO2 fibers were prepared by mixing tetraethyl orthosilicate, ethanol, water and hydrochloric acid. Fibrous SiO2 was drawn by using a viscous solution. Dried gel fibers were final heat-treated at 1000, 1100, 1200 and 1300°C for 1 h in air. Crystallinity of the SiO2 fib...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of materials science 2004-03, Vol.39 (5), p.1683-1687
Hauptverfasser: HWANG, Kyu-Seog, KWON, Jeong-Tae, OH, Jeong-Sun, AN, Jun-Hyung, KIM, Byung-Hoon
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:In this study, sol-gel derived SiO2 fibers were prepared by mixing tetraethyl orthosilicate, ethanol, water and hydrochloric acid. Fibrous SiO2 was drawn by using a viscous solution. Dried gel fibers were final heat-treated at 1000, 1100, 1200 and 1300°C for 1 h in air. Crystallinity of the SiO2 fiber after annealing was measured by X-ray diffraction analysis. A field emission—scanning electron microscope and an atomic force microscope were used to evaluate surface properties. SiO2 fiber heat-treated at high temperature, i.e., 1300°C, exhibited inhomogeneous surface structure.
ISSN:0022-2461
1573-4803
DOI:10.1023/B:JMSC.0000016170.37373.52