Rubber-mortar composites: Effect of composition on properties

The Weibull modulus of mortar specimens containing 35% (w/w of cement content) of NaOH-treated rubber particles was calculated showing a value of 9.1 for the control and 9.4 for the specimens with rubber, indicating that the incorporation of a high amount of rubber does not change the casting reprod...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of materials science 2004-05, Vol.39 (10), p.3319-3327
Hauptverfasser: Segre, N, Joekes, I, Galves, A. D, Rodrigues, J. A
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The Weibull modulus of mortar specimens containing 35% (w/w of cement content) of NaOH-treated rubber particles was calculated showing a value of 9.1 for the control and 9.4 for the specimens with rubber, indicating that the incorporation of a high amount of rubber does not change the casting reproducibility. Since the flexural strength of these rubber-containing specimens was reduced by 43%, new composites were prepared using 10% of rubber as addition or aggregate. Water sorption by immersion, resistance to acid attack, flexural strength and freeze-thaw experiments were performed. Transport properties were improved for the addition-rubber-containing composites; the best results were obtained with the aggregate-rubber-containing composites. A reduction of 15% in flexural strength was observed for addition-rubber-containing composites and 25% for the aggregate-rubber-containing composites, roughly as expected if the flexural strength varies linearly with the rubber content. Furthermore, after 60 freezing and thawing cycles, a reduction of 75% in flexural strength was observed for the control specimens and only 20% for the addition-rubber-containing specimens.
ISSN:0022-2461
1573-4803
DOI:10.1023/B:JMSC.0000026932.06653.de