Infrared fibers based on Te–As–Se glass system with low optical losses

Unclad optical fibers based on high-purity Te–As–Se glasses prepared by chemical and physical methods of purification have been drawn. The optical, thermal and mechanical properties of glasses and fibers were investigated. The minimum optical losses were 0.07 dB/m at 7.3 μm for Te 25As 40Se 35 glass...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of non-crystalline solids 2004-05, Vol.336 (2), p.113-119
Hauptverfasser: Shiryaev, V.S., Adam, J.-L., Zhang, X.H., Boussard-Plédel, C., Lucas, J., Churbanov, M.F.
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Unclad optical fibers based on high-purity Te–As–Se glasses prepared by chemical and physical methods of purification have been drawn. The optical, thermal and mechanical properties of glasses and fibers were investigated. The minimum optical losses were 0.07 dB/m at 7.3 μm for Te 25As 40Se 35 glass fiber and 0.04 dB/m at 6.7 μm for Te 20As 30Se 50 glass fiber. Sixty five percent of input power of a tunable CO 2 laser emitting at 9.3 μm was transmitted through a 1 m long fiber with diameter of 900 μm.