Ultra-shallow junctions produced by plasma doping and flash lamp annealing

The capabilities of plasma doping (PLAD) and flash lamp annealing (FLA) for use in ultra-shallow junction (USJ) fabrication have been evaluated. Silicon wafers have been doped in a BF 3 plasma using wafer biases ranging from 0.6 to 1 kV and a dose of 4 × 10 15 cm −2. The wafers so implanted have bee...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Materials science & engineering. B, Solid-state materials for advanced technology Solid-state materials for advanced technology, 2004-12, Vol.114, p.358-361
Hauptverfasser: Skorupa, Wolfgang, Yankov, Rossen A., Anwand, Wolfgang, Voelskow, Matthias, Gebel, Thoralf, Downey, Daniel F., Arevalo, Edwin A.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The capabilities of plasma doping (PLAD) and flash lamp annealing (FLA) for use in ultra-shallow junction (USJ) fabrication have been evaluated. Silicon wafers have been doped in a BF 3 plasma using wafer biases ranging from 0.6 to 1 kV and a dose of 4 × 10 15 cm −2. The wafers so implanted have been heat-treated by FLA using pre-heating temperatures in the range of 500–700 °C, peak temperatures of 1100–1350 °C, and effective anneal times of 20 and 3 ms. Secondary ion mass spectrometry (SIMS) and sheet resistance measurements have been undertaken to determine the junction depth and the sheet resistance, respectively. Optimum processing conditions have been identified under which both high electrical activation and insignificant dopant diffusion occur compared to the as-implanted state. In this way, one can obtain combinations of junction depth and sheet resistance that meet the 45 nm technology node requirements.
ISSN:0921-5107
1873-4944
DOI:10.1016/j.mseb.2004.07.063