Acid leaching of Turkish celestite concentrate

The grade of final celestite concentrate is as high as 95–96% after jigging and table washing operations applied by Barit Maden Turk in Turkey. Celestite concentrate contains 95% SrSO 4, and 3% CaSO 4, 0.5%BaSO 4, 0.5% SiO 2, 0.5%Fe 2O 3 as major impurities. Before the conversion of celestite to str...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Hydrometallurgy 2004, Vol.71 (3), p.379-383
Hauptverfasser: Dogan, Hacer, Koral, Murat, Kocakusak, Sidika
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The grade of final celestite concentrate is as high as 95–96% after jigging and table washing operations applied by Barit Maden Turk in Turkey. Celestite concentrate contains 95% SrSO 4, and 3% CaSO 4, 0.5%BaSO 4, 0.5% SiO 2, 0.5%Fe 2O 3 as major impurities. Before the conversion of celestite to strontium carbonate with the double decomposition method, the iron content of celestite must be decreased to below 0.10 g/L. This study concerns the acid leaching of Turkish celestite concentrate. A purity of celestite of 98% could be obtained using 50% H 2SO 4 and 1–3% HNO 3 at 40–50 °C and the content of the impurities is about 0.005% Fe, 0.11% Ca, 0.6% Ba, 0.086% Pb and 0.2% others. Strontium carbonate produced from cleaned celestite ore by the method of double decomposition contained iron below 0.10 g/L and calcium below 0.2%.
ISSN:0304-386X
1879-1158
DOI:10.1016/S0304-386X(03)00089-6