The second phases in a burn resistant stable beta titanium alloy-Ti40

The second phases in Ti40 (Ti25V-15Cr-0.2Si) burn resistant titanium alloy are studied. The higher solution temperature, the more second phases in Ti40 alloy. There are not second phases if the solution temperature is below 850°C, while there are rod-like α and little Ti5Si3 phases if temperature is...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of materials science 2003-04, Vol.38 (7), p.1579-1584
Hauptverfasser: ZHAO, Y. Q, QU, H. L, ZHU, K. Y, WU, H, ZHOU, L
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The second phases in Ti40 (Ti25V-15Cr-0.2Si) burn resistant titanium alloy are studied. The higher solution temperature, the more second phases in Ti40 alloy. There are not second phases if the solution temperature is below 850°C, while there are rod-like α and little Ti5Si3 phases if temperature is over 850°C. α, Ti5Si3 and oblique α′′ phases emerge after Ti40 solution at 910°C followed by aging at 600°C, while only Ti5Si3 phases emerge after solution at 860°C followed by aging at 600°C. The effect of the second phases on properties at RT are not obvious. There are different shapes of α and Ti5Si3 precipitates after Ti40 alloy exposure at 540°C for 100 h, which decreases the thermal stability.
ISSN:0022-2461