The effect of cooling rate on structure and properties of a HSLA forging
The mechanical properties along with microstructures of HSLA-80 steel, forged in two stages and subsequently cooled at three different cooling rates, were studied. The fastest cooling rate produced maximum strength due to formation of fine bainite and martensite where as intermediate cooling rate re...
Gespeichert in:
Veröffentlicht in: | Scripta materialia 2003-01, Vol.48 (1), p.51-57 |
---|---|
Hauptverfasser: | , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The mechanical properties along with microstructures of HSLA-80 steel, forged in two stages and subsequently cooled at three different cooling rates, were studied. The fastest cooling rate produced maximum strength due to formation of fine bainite and martensite where as intermediate cooling rate resulted in maximum toughness values owing to predominantly bainitic microstructure. |
---|---|
ISSN: | 1359-6462 1872-8456 |
DOI: | 10.1016/S1359-6462(02)00345-7 |