Diffusivity, activity and solubility of oxygen in liquid lead and lead–bismuth eutectic alloy by electrochemical methods

The diffusivity of oxygen in liquid lead and lead–bismuth eutectic (LBE) alloy was measured by a potentiostatic method and is given by log ( D O Pb / cm 2 s - 1 ) = - 2.554 - 2384 / T ( ± 0.070 ) , 818–1061 K, and log ( D O LBE / cm 2 s - 1 ) = - 0.813 - 3612 / T ( ± 0.091 ) , 811–980 K. The activit...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of nuclear materials 2006-02, Vol.349 (1), p.133-149
Hauptverfasser: Ganesan, Rajesh, Gnanasekaran, T., Srinivasa, Raman S.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The diffusivity of oxygen in liquid lead and lead–bismuth eutectic (LBE) alloy was measured by a potentiostatic method and is given by log ( D O Pb / cm 2 s - 1 ) = - 2.554 - 2384 / T ( ± 0.070 ) , 818–1061 K, and log ( D O LBE / cm 2 s - 1 ) = - 0.813 - 3612 / T ( ± 0.091 ) , 811–980 K. The activity of oxygen in lead and LBE was determined by coulometric titration experiments. Using the measured data, the standard free energy of dissolution of oxygen in liquid lead and LBE was derived and is given by G O ( Pb ) xs = - 121 349 + 16.906 T ( ± 560 ) J ( g atom O ) - 1 , 815 – 1090 K , G O ( LBE ) xs = - 127 398 + 27.938 T ( ± 717 ) J ( g atom O ) - 1 , 812 – 1012 K . Using the above data, the Gibbs energy of formation of PbO(s) and equilibrium oxygen pressures measured over the oxygen-saturated LBE alloy, the solubility of oxygen in liquid lead and LBE were derived. The solubility of oxygen in liquid lead and LBE are given by log( S/at.%O) = −5100/ T + 4.32 (±0.04), 815–1090 K and log( S/at.%O) = −4287/ T + 3.53 (±0.06), 812–1012 K respectively.
ISSN:0022-3115