Rates and product properties of polyethylene produced by copolymerization of 1-hexene and ethylene in the gas phase with ( n-BuCp) 2ZrCl 2 on supports with different pore sizes

The effects of catalyst support pore size and reaction conditions ( T=40–100 °C; ethylene pressure=1.4 MPa; 1-hexene concentration=0–47 mol/m 3) on gas-phase polymerization rates and product properties were studied. Catalysts were prepared by impregnation of mesoporous molecular sieves (pore sizes o...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Polymer (Guilford) 2003-08, Vol.44 (17), p.4791-4803
Hauptverfasser: Kumkaew, P., Wu, L., Praserthdam, P., Wanke, S.E.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The effects of catalyst support pore size and reaction conditions ( T=40–100 °C; ethylene pressure=1.4 MPa; 1-hexene concentration=0–47 mol/m 3) on gas-phase polymerization rates and product properties were studied. Catalysts were prepared by impregnation of mesoporous molecular sieves (pore sizes of 2.5–20 nm) with methylaluminoxane and ( n-BuCp) 2ZrCl 2. Temperature rising elution fractionation, differential scanning calorimetry and size exclusion chromatography were used to characterize the products. The results showed that these catalysts contained multiple types of catalytic sites and that the types of sites were a strong function of the support pore size. Ethylene polymerization and 1-hexene incorporation rates were strong functions of support pore size, 1-hexene concentration, and temperature. Large-pored catalysts had higher 1-hexene incorporation rates and the rate of 1-hexene incorporation was a function of polymerization time. Highest polymerization rates were obtained at 80 °C and 1-hexene concentration of 4–12 mol/m 3; high 1-hexene concentrations resulted in large decreases in polymerization rates.
ISSN:0032-3861
1873-2291