Preparation of Dense MgB2 Bulk Superconductors by Spark Plasma Sintering

Fully dense MgB2 bulk specimens (∼higher than 99% dense) were prepared using spark plasma sintering (SPS) at 1250°C for 15 min. Microstructure analyses revealed that faceted MgO particles of ∼8% volume fraction were dispersed in the MgB2 matrix. A sharp superconducting transition with an onset tempe...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of the American Ceramic Society 2003-10, Vol.86 (10), p.1800-1802
Hauptverfasser: Lee, Soo-Yong, Yoo, Sang-Im, Kim, Young-Woon, Hwang, Nong M., Kim, Doh-Yeon
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Fully dense MgB2 bulk specimens (∼higher than 99% dense) were prepared using spark plasma sintering (SPS) at 1250°C for 15 min. Microstructure analyses revealed that faceted MgO particles of ∼8% volume fraction were dispersed in the MgB2 matrix. A sharp superconducting transition with an onset temperature of 38.5 K was confirmed by both magnetization and resistivity measurements.