Ultra-thin Cr2O3 well-crystallized films for high transmittance APSM in ArF line
Ultra-thin Cr2O3 well-crystallized thin films are deposited on UV grade fused silica substrates and Si wafers by using r.f. reactive unbalanced magnetron sputtering from a Cr metal target in an atmosphere of Ar and (X at 350DGC. The optical constants of such thin films were found to be a sensitive f...
Gespeichert in:
Veröffentlicht in: | Microelectronic engineering 2003-06, Vol.67-68, p.17-23 |
---|---|
Hauptverfasser: | , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Ultra-thin Cr2O3 well-crystallized thin films are deposited on UV grade fused silica substrates and Si wafers by using r.f. reactive unbalanced magnetron sputtering from a Cr metal target in an atmosphere of Ar and (X at 350DGC. The optical constants of such thin films were found to be a sensitive function of oxygen-to-argon flow rate ratio. At the ratio of 0.2, a Cr2O, well-crystallized thin film with appropriate refractive index and extinction coefficient at a wavelength of 365 nm can be used as attenuated phase-shifting mask (APSM) blank as well as being good for inspection. The simulated thickness range of a Cr2O3 well-crystallized thin film was found to be between 28.2 and 30.3 nm. This meets the optical requirements for high transmittance APSM (HT-APSM) with a transmittance of 18-20% at 193 nm for the pattern fabrication and with transmittance less than 50% at 365 nm for the mask inspection. One such Cr2O3 well-crystallized thin film that satisfies the optical requirements was fabricated. |
---|---|
ISSN: | 0167-9317 1873-5568 |
DOI: | 10.1016/S0167-9317(03)00179-5 |