Nickel-molybdenum catalysts fabricated by mechanical alloying and spark plasma sintering

The low energy ball milling process has been used to fabricate Ni–43at.%Mo based electro-active powder. Nanometre-sized Mo particles have been embedded into an agglomerated amorphous matrix. The spark plasma sintering (SPS) process has been used to densify the powder in

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Materials science & engineering. A, Structural materials : properties, microstructure and processing Structural materials : properties, microstructure and processing, 2000-01, Vol.276 (1), p.226-235
Hauptverfasser: De la Torre, S.D., Oleszak, D., Kakitsuji, A., Miyamoto, K., Miyamoto, H., Martı́nez-S., R., Almeraya-C, F., Martı́nez-V., A., Rios-J., D.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The low energy ball milling process has been used to fabricate Ni–43at.%Mo based electro-active powder. Nanometre-sized Mo particles have been embedded into an agglomerated amorphous matrix. The spark plasma sintering (SPS) process has been used to densify the powder in
ISSN:0921-5093
1873-4936
DOI:10.1016/S0921-5093(99)00156-2