Grain size effects on the magnetic properties of chemically synthesized Ni:Ni sub(3)C nanocomposites

The synthesis of Ni:Ni sub(3)C nanocomposites with grain sizes from 5 to 60 nm and Ni sub(3)C nanocomposites with grain sizes from 20 to 50 nm. are described. The room-temperature coercivity and remanence ration are measured in terms of Ni grain size. Room-temperature measurements show that the Ni s...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of magnetism and magnetic materials 2000-12, Vol.222 (1-2), p.70-78
Hauptverfasser: Bonder, M J, Kirkpatrick, E M, Martin, T, Kim, S-J, Rieke, R D, Leslie-Pelecky, Diandra L
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The synthesis of Ni:Ni sub(3)C nanocomposites with grain sizes from 5 to 60 nm and Ni sub(3)C nanocomposites with grain sizes from 20 to 50 nm. are described. The room-temperature coercivity and remanence ration are measured in terms of Ni grain size. Room-temperature measurements show that the Ni sub(3)C affect the collective magnetic behavior through interactions of the Ni particles.
ISSN:0304-8853