Effect of addition of reprocessed nylon 6 with virgin material for roller assembly used in printers

This work is aimed at optimizing the percentage of reprocessed nylon 6 that can be added with virgin nylon 6 without undue sacrifice in properties. The effect of annealing on various properties such as tensile strength, impact strength, hardness, heat deflection temperature, abrasion resistance, and...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of applied polymer science 2000-12, Vol.78 (10), p.1737-1743
Hauptverfasser: Vinay, M. N., Ravishankar, S., Girish, T. P., Radhakrishnan, R., Ananthapadmanabha, G. S., Shashidhara, G. M.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:This work is aimed at optimizing the percentage of reprocessed nylon 6 that can be added with virgin nylon 6 without undue sacrifice in properties. The effect of annealing on various properties such as tensile strength, impact strength, hardness, heat deflection temperature, abrasion resistance, and dimensional variation are studied. The annealed samples of 70/30 composition (virgin/reprocessed) have shown remarkable improvement in mechanical strength when compared to nonannealed samples. Thus a costly material like polyacetal, which is used to make critical roller components of printers, may be replaced by less costlier nylon 6 with recommended proportion of regrind without affecting the desired properties. © 2000 John Wiley & Sons, Inc. J Appl Polym Sci 78: 1737–1743, 2000
ISSN:0021-8995
1097-4628
DOI:10.1002/1097-4628(20001205)78:10<1737::AID-APP40>3.0.CO;2-W