Effect of cold-rolling on magnetic properties of non-oriented silicon steel sheets (Part II)
Non-oriented 3% Si–Fe sheet with strong primary recrystallization texture of (1 0 0)[0 0 1] was made through the process of cross cold-rolling, one-stage intermediate annealing, and final annealing at 900°C for 1.5 h.
Gespeichert in:
Veröffentlicht in: | Journal of magnetism and magnetic materials 2000-02, Vol.209 (1), p.197-200 |
---|---|
Hauptverfasser: | , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Non-oriented 3% Si–Fe sheet with strong primary recrystallization texture of (1
0
0)[0
0
1] was made through the process of cross cold-rolling, one-stage intermediate annealing, and final annealing at 900°C for 1.5
h. |
---|---|