Amounts of Sn and Pd Absorbed by Pretreatment for Electroless Deposition and Surface Morphology of Co-P Deposits

In regard to magnetic disks when magnetic layer is formed on a glass substrate using electroless method, it is necessary to carry out pretreatment to give catalytic properties to the substrate. This is the sensitizing activating method which is used by authors to measure the properties of absorbed m...