Thick amorphous ferromagnetic coatings via thermal spraying of spark-eroded powder
300-μm thick amorphous ferromagnetic coatings were prepared by thermally spraying amorphous Fe 75Si 15B 10 powder. The amorphous feedstock powder for the thermal spraying was made by the spark-erosion method. The Mössbauer, X-ray diffraction, chemical, and magnetic properties of the coatings were ve...
Gespeichert in:
Veröffentlicht in: | Materials letters 2001-04, Vol.48 (3), p.184-187 |
---|---|
Hauptverfasser: | , , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | 300-μm thick amorphous ferromagnetic coatings were prepared by thermally spraying amorphous Fe
75Si
15B
10 powder. The amorphous feedstock powder for the thermal spraying was made by the spark-erosion method. The Mössbauer, X-ray diffraction, chemical, and magnetic properties of the coatings were very similar to those of the spark-eroded powder. Consolidated magnetic amorphous materials have long been a technological goal, and are expected to provide substantial electrical energy savings. |
---|---|