Evidence for the transport of impurity hydrogen with gliding dislocations in aluminum
A tritiated pure aluminum specimen was autoradiographically processed with a plastic strain of 5% prior to exposure. Microscopic autoradiographs revealed a clear evidence for hydrogen transport with gliding dislocations: an array of silver particles, i.e. tritium, was evident on the slip steps on th...
Gespeichert in:
Veröffentlicht in: | Scripta Materialia 1996-09, Vol.35 (6), p.695-698 |
---|---|
Hauptverfasser: | , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A tritiated pure aluminum specimen was autoradiographically processed with a plastic strain of 5% prior to exposure. Microscopic autoradiographs revealed a clear evidence for hydrogen transport with gliding dislocations: an array of silver particles, i.e. tritium, was evident on the slip steps on the specimen surface. |
---|---|
ISSN: | 1359-6462 1872-8456 |
DOI: | 10.1016/1359-6462(96)00200-X |