Effect of aromatic diamine extenders on the morphology and property of RIM polyurethane-urea
An aromatic diamine, CMOMDA, was synthesized and used as a chain extender for reaction injection molding (RIM) polyurethane–urea. The morphology and properties of CMOMDA‐, DETDA‐, and MDA‐extended poly(ether–urethane–urea)s (PEUUs) were measured by IR, DSC, DMS, SEM, and tensile testing apparatus. W...
Gespeichert in:
Veröffentlicht in: | Journal of applied polymer science 1994-07, Vol.53 (1), p.23-29 |
---|---|
Hauptverfasser: | , , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | An aromatic diamine, CMOMDA, was synthesized and used as a chain extender for reaction injection molding (RIM) polyurethane–urea. The morphology and properties of CMOMDA‐, DETDA‐, and MDA‐extended poly(ether–urethane–urea)s (PEUUs) were measured by IR, DSC, DMS, SEM, and tensile testing apparatus. Well‐matched values of
C
h
and
X
ut,b
/
C
h
were necessary for aromatic diamine‐extended PEUU. DSC and SEM showed that the aggregation state of hard segments might undergo some changes with increasing hard‐segment content. © 1994 John Wiley & Sons, Inc. |
---|---|
ISSN: | 0021-8995 1097-4628 |
DOI: | 10.1002/app.1994.070530103 |