Spinodal decomposition in Fe9.0Al30.5MnxC alloys

The as-quenched microstructure of iron)aluminum)manganese)carbon alloys with high C contents was investigated. Two Fe alloys containing 9% Al and 30.5% Mn were produced. Alloy A contained 1.36% C and alloy B contained 2.02% C. After air induction melting the alloys were hot forged and cold rolled to...