Effect of different preparation finishing procedures on the marginal and internal fit of CAD-CAM-produced restorations: A microcomputed tomography evaluation

Accurate fit is an important factor for the longevity of computer-aided design and computer-aided manufacturing (CAD-CAM) ceramic restorations. Few studies have compared how restoration finishing procedures affect the marginal and internal fit of these restorations by using microcomputed tomography...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:The Journal of prosthetic dentistry 2023-10, Vol.130 (4), p.605-610
Hauptverfasser: Tamam, Evşen, Bankoğlu Güngör, Merve, Karakoca Nemli, Seçil, Bilecenoğlu, Burak, Ocak, Mert
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Accurate fit is an important factor for the longevity of computer-aided design and computer-aided manufacturing (CAD-CAM) ceramic restorations. Few studies have compared how restoration finishing procedures affect the marginal and internal fit of these restorations by using microcomputed tomography (μCT). The purpose of this in vitro study was to evaluate the preparations with different surface finishing procedures for the fit of CAD-CAM restorations by using μCT. A total of 28 anatomic contour monolithic feldspathic ceramic crowns were produced for 4 typodont teeth prepared according to the different surface finishing procedures (n=7). The generated experimental groups were finishing with extra-coarse (181 μm) diamond rotary instruments (EC), finishing with fine (40 μm) diamond rotary instruments after extra-coarse diamond rotary instruments (F), finishing with very fine (20 μm) diamond rotary instruments after extra-coarse and fine diamond rotary instruments (VF), and finishing with extra-coarse, fine, and very fine diamond rotary instruments followed by polishing rubber points (P). μCT scans were obtained to measure the gaps between the typodont teeth and the crowns. Reference points such as the margin, chamfer (the deepest point), cusp tips, and central fossa were determined, and 196 measurements were made. Data were analyzed by using 2-way analyses of variance and the Tukey HSD test (α=.05). The highest gap values in all sections were observed in the finishing with extra-coarse (181 μm) diamond rotary instruments group. The lowest gap value in the marginal point was observed in the P group (P