Cylindrical ingots of the alloy Nd 17Fe 76.5B 5Cu 1.5 were upset forged in a crank press at an average strain rate of 0.8 s −1 at temperatures of 750, 850 and 950°C. Microstructural development and magnetic properties are treated in terms of the material flow during the semi-solid deformation of the...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of alloys and compounds 1995-11, Vol.230 (1), p.42-45
Hauptverfasser: Sinka, V., Kvacˇkaj, T., Assis, O.B.G., Ferrante, M.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Cylindrical ingots of the alloy Nd 17Fe 76.5B 5Cu 1.5 were upset forged in a crank press at an average strain rate of 0.8 s −1 at temperatures of 750, 850 and 950°C. Microstructural development and magnetic properties are treated in terms of the material flow during the semi-solid deformation of the alloy as a function of the forging temperature. The results indicate increasing microstructural inhomogeneity due to the compaction flow at higher forging temperatures.