Fatigue‐Resistant Interfacial Layer for Safe Lithium Metal Batteries
The plating/stripping of Li dendrites can fracture the static solid electrolyte interphase (SEI) and cause significant dynamic volume variations in the Li anode, which give rise to poor cyclability and severe safety hazards. Herein, a tough polymer with a slide‐ring structure was designed as a self‐...
Gespeichert in:
Veröffentlicht in: | Angewandte Chemie International Edition 2021-11, Vol.60 (48), p.25508-25513 |
---|---|
Hauptverfasser: | , , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The plating/stripping of Li dendrites can fracture the static solid electrolyte interphase (SEI) and cause significant dynamic volume variations in the Li anode, which give rise to poor cyclability and severe safety hazards. Herein, a tough polymer with a slide‐ring structure was designed as a self‐adaptive interfacial layer for Li anodes. The slide‐ring polymer with a dynamically crosslinked network moves freely while maintaining its toughness and fracture resistance, which allows it can to dissipate the tension induced by Li dendrites on the interphase layer. Moreover, the slide‐ring polymer is highly stretchable, elastic, and displays an ultrafast self‐healing ability, which allows even pulverized Li to remain coalesced without disintegrating upon consecutive cycling. The Li anodes demonstrate greatly improved suppression of Li dendrite formation, as evidenced by the high critical current density (6 mA cm−2) and stable cycling for the full cells with high‐areal capacity LiFePO4, high‐voltage NCM, and S cathodes.
A slide‐ring polymer with a high stiffness, high toughness and excellent fracture resistance is designed to adapt its shape to dynamic electrode volume variations and stabilize the lithium anode upon cycling. |
---|---|