Hydrogen-induced disproportionation of the intermetallic compound ZrCo
Disproportionation of the intermetallic compound ZrCo in the presence of hydrogen into ZrH sub 2 and ZrCo sub 2 has been observed in the temperature range 350-500 deg C during both the absorption and the desorption mode. Quantitative reproportionation into ZrCo can be achieved by vacuum annealing at...
Gespeichert in:
Veröffentlicht in: | Chemistry of materials 1992-05, Vol.4 (3), p.631-639 |
---|---|
Hauptverfasser: | , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Disproportionation of the intermetallic compound ZrCo in the presence of hydrogen into ZrH sub 2 and ZrCo sub 2 has been observed in the temperature range 350-500 deg C during both the absorption and the desorption mode. Quantitative reproportionation into ZrCo can be achieved by vacuum annealing at high temperatures. The resistance of a sample toward degradation was found to be determined by its previous history. |
---|---|
ISSN: | 0897-4756 1520-5002 |
DOI: | 10.1021/cm00021a025 |