Develop spinel structure and quantify phase transformation for nickel stabilization in electroplating sludge

Ni in the electroplating sludge can be incorporated into NiFe2O4 and NiAl2O4 spinel structures, when two typical ceramic precursors (α-Fe2O3 and γ-Al2O3) were used respectively. The transformation ratio of Ni into the either spinel can reach over 99%. The two spinels exhibit superiority in Ni stabil...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Waste management (Elmsford) 2021-07, Vol.131, p.286-293
Hauptverfasser: Xia, Yunxue, Meng, Fanling, Lv, Zhong, Zhang, Jianshuai, Tang, Yuanyuan, Shih, Kaimin
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Ni in the electroplating sludge can be incorporated into NiFe2O4 and NiAl2O4 spinel structures, when two typical ceramic precursors (α-Fe2O3 and γ-Al2O3) were used respectively. The transformation ratio of Ni into the either spinel can reach over 99%. The two spinels exhibit superiority in Ni stabilization with leached ratio of
ISSN:0956-053X
1879-2456
DOI:10.1016/j.wasman.2021.06.019