Shear Bond Strength of Different MDP-Containing Adhesive Systems on Enamel and Dentin from Primary Teeth

Objective: To compare the shear bond strength (SBS) after thermocycling of four universal adhesives applied in self-etch mode on dentin and etch-and-rinse mode on enamel. Study design: Flat 144 buccal or lingual dentin and enamel surfaces from 72 non-carious primary molars were prepared. Samples wer...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:The Journal of clinical pediatric dentistry 2021-07, Vol.45 (3), p.186-192
Hauptverfasser: Kim, Min Jin, Kim, Joonhee, Song, Ji-Soo, Chung, Shin Hye, Hyun, Hong-Keun
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Objective: To compare the shear bond strength (SBS) after thermocycling of four universal adhesives applied in self-etch mode on dentin and etch-and-rinse mode on enamel. Study design: Flat 144 buccal or lingual dentin and enamel surfaces from 72 non-carious primary molars were prepared. Samples were segregated into 12 groups (n=12): Adper Single Bond 2 etch-and-rinse (SB_T) and Clearfil SE Bond self-etch (SE_S) applied to enamel and dentin served as controls. Scotch Bond Universal Adhesive (SBU), Clearfil S3 Bond Universal Adhesive (SEU), Tetric N-Bond Universal Adhesive (TEN), and All Bond Universal (BIS) were applied in etch-and-rinse mode to enamel and in self-etch mode to dentin. They were thermocycled for 5000 cycles. SBS testing and the evaluation of fracture mode were performed. Results: SB_T showed statistically higher SBS than other adhesive groups using etch-and-rinse mode on enamel. SE_S and BIS had statistically higher SBS than other adhesive groups using self-etch mode on dentin. Mixed failure was the most common failure mode in each group. Conclusion: The universal adhesives did not show higher SBS than SB_T when using etch-and-rinse on enamel. All universal adhesives showed higher SBS than SB_T and had SBS similar to SE_S, except SBU when using self-etch mode on dentin.
ISSN:1053-4628
1557-5268
DOI:10.17796/1053-4625-45.3.7