Fabrication of an oxide superconducting wire by a drawing-rolling method
A tape-shaped wire with YBa sub 2 Cu sub 3 O sub 7 core and Ag sheath was fabricated by a drawing--rolling method. The critical current density J sub c apparently depended on the thickness of the tape and increased markedly with decreasing tape thickness. The maximum J sub c of 3330 A/cm exp 2 at 77...
Gespeichert in:
Veröffentlicht in: | Journal of the Japan Society of Powder and Powder Metallurgy 1988, Vol.35 (5), p.325-328 |
---|---|
Hauptverfasser: | , , , , |
Format: | Artikel |
Sprache: | eng ; jpn |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A tape-shaped wire with YBa sub 2 Cu sub 3 O sub 7 core and Ag sheath was fabricated by a drawing--rolling method. The critical current density J sub c apparently depended on the thickness of the tape and increased markedly with decreasing tape thickness. The maximum J sub c of 3330 A/cm exp 2 at 77K in a zero magnetic field was achieved in a tape with 0.06 mm thickness. The presence of a 20 mT magnetic field reduced the J sub c value by 1/100. 8 ref.--AA |
---|---|
ISSN: | 0532-8799 1880-9014 |
DOI: | 10.2497/jjspm.35.325 |