Effects of remaining dentin thickness, smear layer and aging on the bond strengths of self-etch adhesives to dentin

This study evaluated the effects of remaining dentin thickness (RDT), different smear layers, and aging on the microtensile bond strength (µTBS) of universal adhesives to dentin when applied in self-etch mode. Ninety-six human third molars were randomly allocated to 12 groups (n=8) based on adhesive...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Dental Materials Journal 2021/03/25, Vol.40(2), pp.538-546
Hauptverfasser: AKTER, Rime Shamme, AHMED, Zubaer, YAMAUTI, Monica, CARVALHO, Ricardo M., Abu Faem Mohammad Almas CHOWDHURY, SANO, Hidehiko
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:This study evaluated the effects of remaining dentin thickness (RDT), different smear layers, and aging on the microtensile bond strength (µTBS) of universal adhesives to dentin when applied in self-etch mode. Ninety-six human third molars were randomly allocated to 12 groups (n=8) based on adhesives: ClearfilTM SE Bond 2 (SE, control), ClearfilTM Universal Bond (CU) and ScotchBondTM Universal Adhesive (SB); smear layers: prepared either with 600-grit SiC paper (P) or regular diamond bur (B); and aging: stored in distilled water at 37ºC for 24 hours (24h) or 1 year (1y). µTBS was significantly affected by the type of adhesives, smear layers, and aging (p
ISSN:0287-4547
1881-1361
DOI:10.4012/dmj.2019-436