Microarc oxidation surface of titanium implants promote osteogenic differentiation by activating ERK1/2-miR-1827-Osterix
There has been a constant requirement from the clinic to develop biomédical titanium (Ti) implants with high osteogenic ability. In this study, we clarified a novel mechanism of how MAO (microarc oxidation) coating of Ti implants facilitates osteogenic differentiation of human bone marrow mesenchyma...
Gespeichert in:
Veröffentlicht in: | In vitro cellular & developmental biology. Animal 2020-04, Vol.56 (4), p.296-306 |
---|---|
Hauptverfasser: | , , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | There has been a constant requirement from the clinic to develop biomédical titanium (Ti) implants with high osteogenic ability. In this study, we clarified a novel mechanism of how MAO (microarc oxidation) coating of Ti implants facilitates osteogenic differentiation of human bone marrow mesenchymal stem cells (hB-MSCs) by activating ERKl/2-miR-1827-Osterix signaling pathway in vitro. MAO surface of titanium implant was more favorable to promote osteogenic differentiation than SLA and AOS coating. Besides, titanium implants regulated hB-MSCs osteogenesis through the p38 MAPK pathway and ERK1/2 might be the most efficient target. Furthermore, MAO coating induced osteogenic differentiation though ERK1/2-miR-1827 pathway. Finally, we verified miR-1827 regulated osteogenic differentiation partially through Osterix. Our study reveals novel insights that MAO surface of titanium implant is a prior choice for biomédical trial and for its use in periprosthetic osteolysis (PIO) treatment in an evidence-based rationale. |
---|---|
ISSN: | 1071-2690 1543-706X |
DOI: | 10.1007/s11626-020-00444-7 |