Injectable porcine bone demineralized and digested extracellular matrix—PEGDA hydrogel blend for bone regeneration

Extracellular matrix (ECM) has a major role in the structural support and cellular processes of organs and tissues. Proteins extracted from the ECM have been used to fabricate different scaffolds for tissue engineering applications. The aims of the present study were to extract, characterize and fab...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of materials science. Materials in medicine 2020-02, Vol.31 (2), p.21-21, Article 21
Hauptverfasser: Obregon-Miano, Fabian, Fathi, Ali, Rathsam, Catherine, Sandoval, Isbel, Deheghani, Fariba, Spahr, Axel
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Extracellular matrix (ECM) has a major role in the structural support and cellular processes of organs and tissues. Proteins extracted from the ECM have been used to fabricate different scaffolds for tissue engineering applications. The aims of the present study were to extract, characterize and fabricate a new class of hydrogel with proteins isolated from pig bone ECM and combine them with a synthetic polymer so it could be used to promote bone regeneration. Porcine bone demineralized and digested extracellular matrix (pddECM) containing collagen type I was produced, optimized and sterilized with high pressurized CO 2 method. The pddECM was further blended with 20% w/v polyethylene glycol diacrylate (PEGDA) to create an injectable semi interpenetrating polymer network (SIPN) scaffold with enhanced physicochemical properties. The blend tackled the shortfall of natural polymers, such as lack of structural stability and fast degradation, preserving its structure in more than 90% after 30 days of incubation; thus, increasing the material endurance in a simulated physiological environment. The manufactured injectable hydrogel showed high cytocompatibility with hOb and SaOs-2 cells, promoting osteogenic proliferation within 21 days of culture. The hydrogel had a high compression modulus of 520 kPa, low swelling (5.3 mg/mg) and millimetric volume expansion (19.5%), all of which are favorable characteristics for bone regeneration applications.