Sorghum straw: Pulping and bleaching process optimization and synthesis of cellulose acetate
The process employed for the pulping and bleaching of sorghum straw was optimized prior to the synthesis of cellulose acetate. A 22 factorial central composite design was carried out. The variables considered were cooking time (1.5 to 2.5 h) and dilute alkali concentration (0.75 to 1.25%) for the pu...
Gespeichert in:
Veröffentlicht in: | International journal of biological macromolecules 2019-08, Vol.135, p.877-886 |
---|---|
Hauptverfasser: | , , , , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The process employed for the pulping and bleaching of sorghum straw was optimized prior to the synthesis of cellulose acetate. A 22 factorial central composite design was carried out. The variables considered were cooking time (1.5 to 2.5 h) and dilute alkali concentration (0.75 to 1.25%) for the pulping and bleaching time (30 to 35 min) and bleach volume (20 to 25 mL) for the bleaching. The sorghum straw was comprised of 49.43% α-cellulose, 19.18% hemicellulose and 30.42% lignin. The optimum conditions that maximize these processes were 2.5 h and 1.25% (dilute alkali concentration) at 90 °C, and 35 min and 25 mL (bleach volume) at 80 °C, respectively, providing pulps with a low Kappa number ( |
---|---|
ISSN: | 0141-8130 1879-0003 |
DOI: | 10.1016/j.ijbiomac.2019.05.014 |