Viscoelastic stability of pre-cured resin-composite CAD/CAM structures
To study the effect of water storage (3 months) on the creep deformation and recovery of CAD/CAM composite materials to determine their viscoelastic stability. Five CAD/CAM composite blocks, with increasing filler loading, and one polymer-infiltrated ceramic network (PICN) were studied. Six specimen...
Gespeichert in:
Veröffentlicht in: | Dental materials 2019-08, Vol.35 (8), p.1166-1172 |
---|---|
Hauptverfasser: | , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | To study the effect of water storage (3 months) on the creep deformation and recovery of CAD/CAM composite materials to determine their viscoelastic stability.
Five CAD/CAM composite blocks, with increasing filler loading, and one polymer-infiltrated ceramic network (PICN) were studied. Six specimens of each material were separated into two groups (n=3) according to their storage conditions (24 h dry storage at 23°C versus 3 months storage in 37°C distilled water). A constant static compressive stress of 20 MPa was applied on each specimen via a loading pin for 2 h followed by unloading and monitoring strain recovery for a further period of 2 h. The maximum creep-strain (%) and permanent set (%) were recorded. Data were analysed via two-way ANOVA followed by one-way ANOVA and Bonferroni post hoc tests ( |
---|---|
ISSN: | 0109-5641 1879-0097 |
DOI: | 10.1016/j.dental.2019.05.007 |