In-Depth Understanding of the Morphology Effect of α‑Fe2O3 on Catalytic Ethane Destruction

Shape effects of nanocrystal catalysts in different reactions have attracted remarkable attention. In the present work, three types of α-Fe2O3 oxides with different micromorphologies were rationally synthesized via a facile solvothermal method and adopted in deep oxidation of ethane. The physicochem...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:ACS applied materials & interfaces 2019-03, Vol.11 (12), p.11369-11383
Hauptverfasser: Jian, Yanfei, Yu, Tingting, Jiang, Zeyu, Yu, Yanke, Douthwaite, Mark, Liu, Jingyin, Albilali, Reem, He, Chi
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Shape effects of nanocrystal catalysts in different reactions have attracted remarkable attention. In the present work, three types of α-Fe2O3 oxides with different micromorphologies were rationally synthesized via a facile solvothermal method and adopted in deep oxidation of ethane. The physicochemical properties of prepared materials were characterized by XRD, N2 sorption, FE-SEM, HR-TEM, FTIR, in situ DRIFTS, XPS, Mössbauer spectroscopy, in situ Raman, electron energy loss spectroscopy, and H2-TPR. Moreover, the formation energy of oxygen vacancy and surface electronic structure on various crystal faces of α-Fe2O3 were explored by DFT calculations. It is shown that nanosphere-like α-Fe2O3 exhibits much higher ethane destruction activity and reaction stability than nanocube-like α-Fe2O3 and nanorod-like α-Fe2O3 due to larger amounts of oxygen vacancies and lattice defects, which greatly enhance the concentration of reactive oxygen species, oxygen transfer speed, and material redox property. In addition to this, DFT results reveal that nanosphere-like α-Fe2O3 has the lowest formation energy of oxygen vacancy on the (110) facet (E vo (110) = 1.97 eV) and the strongest adsorption energy for ethane (−0.26 eV) and O2 (−1.58 eV), which can accelerate the ethane oxidation process. This study has deepened the understanding of the face-dependent activities of α-Fe2O3 in alkane destruction.