Leaching of Gold and Silver from Crushed Au-Ag Wastes
Au-Ag noble metal wastes represent a wide range of waste types and forms with various ballast elements and components. The thiourea process of gold and silver extraction from ores, concentrates or secondary raw materials consists of gold and silver leaching into the thiourea solution and the consequ...
Gespeichert in:
Veröffentlicht in: | The open chemical engineering journal 2008-02, Vol.2 (1), p.6-9 |
---|---|
Hauptverfasser: | , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Au-Ag noble metal wastes represent a wide range of waste types and forms with various ballast elements and
components. The thiourea process of gold and silver extraction from ores, concentrates or secondary raw materials consists
of gold and silver leaching into the thiourea solution and the consequent precipitation of these metals from the solution.
Due to the non-toxic character of thiourea it is the perspective alternative to the up to now most frequently used cyanide
method. The thiourea leaching of gold and silver from electronic waste, goldsmith’s waste and ceramic waste using
crushing as the pretreatment step was investigated. For electronic waste, it was possible to achieve 97 % gold and 94 %
silver recovery within 120 minutes of thiourea leaching. Up to 98 % of gold and 96 % of silver were recovered from goldsmith’s
waste after 60 minutes of leaching. In the case of ceramic waste, we achieved up to 98 % gold and 97 % silver extraction
efficiency after only 45 minutes of leaching. In comparison with the classical cyanide leaching, thiourea leaching
acts faster and without a harmful environmental impact. |
---|---|