Highly Sensitive, Temperature-Independent Oxygen Gas Sensor Based on Anatase TiO2 Nanoparticle Grafted, 2D Mixed Valent VO x Nanoflakelets

Herein, we report a facile approach for the synthesis of TiO2 nanoparticles tethered on 2D mixed valent vanadium oxide (VO x /TiO2) nanoflakelets using a thermal decomposition assisted hydrothermal method and investigation of its temperature-independent performance enhancement in oxygen-sensing prop...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:ACS sensors 2018-09, Vol.3 (9), p.1811-1821
Hauptverfasser: Raghu, Appu Vengattoor, Karuppanan, Karthikeyan K, Pullithadathil, Biji
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Herein, we report a facile approach for the synthesis of TiO2 nanoparticles tethered on 2D mixed valent vanadium oxide (VO x /TiO2) nanoflakelets using a thermal decomposition assisted hydrothermal method and investigation of its temperature-independent performance enhancement in oxygen-sensing properties. The material was structurally characterized using XRD, TEM, Raman, DSC, and XPS analysis. The presence of mixed valent states, such as V2O5 and VO2 in VO x , and the metastable properties of VO2 have been found to play crucial roles in the temperature-independent electrical conductivity of VO x /TiO2 nanoflakelets. Though pristine VO x exhibited characteristic semiconductor-to-metal transition of monoclinic VO2, pure VO x nanoflakelets exhibited poor sensitivity toward sensing oxygen. VO x /TiO2 nanoflakelets showed a very low temperature coefficient of resistance above 150 °C with improved sensitivity (35 times higher than VO x for 100 ppm) toward oxygen gas. VO x /TiO2 nanoflakelets exhibited much higher response, faster adsorption and desorption toward oxygen as compared to pristine VO x beyond 100 °C, which endowed the sensor with excellent temperature-independent sensor properties within 150–500 °C. The faster adsorption and desorption after 100 °C led to shorter response time (3–5 s) and recovery time (7–9 s). The results suggest that 2D VO x /TiO2 can be a promising candidate for temperature-independent oxygen sensor applications.