Nuclear penetration of surface functionalized gold nanoparticles
Free gold nanoparticles easily aggregate when the environment conditions change. Here, gold nanoparticles (AuNPs) with average diameter of 3.7 nm were prepared and then modified with poly(ethylene glycol) (PEG) to improve stability. The gold nanoparticles were first surface-modified with 3-mercaptop...
Gespeichert in:
Veröffentlicht in: | Toxicology and applied pharmacology 2009-06, Vol.237 (2), p.196-204 |
---|---|
Hauptverfasser: | , , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Free gold nanoparticles easily aggregate when the environment conditions change. Here, gold nanoparticles (AuNPs) with average diameter of 3.7 nm were prepared and then modified with poly(ethylene glycol) (PEG) to improve stability. The gold nanoparticles were first surface-modified with 3-mercaptopropionic acid (MPA) to form a self-assembled monolayer and subsequently conjugated with NH
2-PEG-NH
2 through amidation between the amine end groups on PEG and the carboxylic acid groups on the particles. The biocompatibility and intracellular fate of PEG-modified gold nanoparticles (AuNP@MPA-PEG) were then studied in human cervical cancer (HeLa) cells. Cell viability test showed that AuNP@MPA-PEG did not induce obvious cytotoxicity. Both confocal laser scanning microscopy and transmission electron microscopy demonstrated that AuNP@MPA-PEG entered into mammalian cells and the cellular uptake of AuNP@MPA-PEG was time-dependent. Inductively coupled plasma mass spectrometry and confocal microscopy imaging further demonstrated that AuNP@MPA-PEG penetrated into the nucleus of mammalian cells upon exposure for 24 h. These results suggest that surface modification can enhance the stability and improve the biocompatibility. This study also indicates that AuNP@MPA-PEG can be used as potential nuclear targeted drug delivery carrier. |
---|---|
ISSN: | 0041-008X 1096-0333 |