Biomechanical comparison of three kinds of fixation instruments for calcaneal osteotomy

To compare the biomechanical characteristics of self-made nickel-titanium shape memory alloy stepped plate with calcaneal plate and cannulated compression screws in fixing calcaneal osteotomy. Calcaneal osteotomy was operated on 6 fresh-frozen lower limbs collected from donors. Then three kinds of f...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Zhongguo xiu fu chong jian wai ke za zhi 2018-02, Vol.32 (2), p.192
Hauptverfasser: Bai, Jiyue, Xu, Yongqing, He, Xiaoqing, Li, Chuan, Liu, Shuai, Li, Liang
Format: Artikel
Sprache:chi
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:To compare the biomechanical characteristics of self-made nickel-titanium shape memory alloy stepped plate with calcaneal plate and cannulated compression screws in fixing calcaneal osteotomy. Calcaneal osteotomy was operated on 6 fresh-frozen lower limbs collected from donors. Then three kinds of fixation materials were applied in random, including the self-made nickel-titanium shape memory alloy stepped plate (group A), calcaneal plate (group B), and cannulated compression screws (group C). Immediately after fixation, axial loading of 20-600 N and 20 N/s in speed was introduced to record the biomechanical data including maximum displacement, elastic displacement, and maximum load. Then fatigue test was performed (5 Hz in frequency and repeat 3 000 times) and the same axial loading was introduced to collect the biomechanical data. Finally, the axial compression stiffness before and after fatigue test were calculated. There was no significant difference in the axial compression stiffness between pre- and post
ISSN:1002-1892
DOI:10.7507/1002-1892.201709121