Insight into the H2S selective catalytic oxidation performance on well-mixed Ce-containing rare earth catalysts derived from MgAlCe layered double hydroxides

[Display omitted] •The MgAlCeO rare earth catalysts exhibited excellent catalytic activities.•No chemisorption O vacancies existed on catalyst surface.•The MgAlCeO rare earth catalysts obeyed a step-wise mechanism.•The effect of added water was investigated deeply. A series of well-mixed Ce-containi...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of hazardous materials 2018-01, Vol.342, p.749-757
Hauptverfasser: Zhang, Fenglian, Zhang, Xin, Hao, Zhengping, Jiang, Guoxia, Yang, Hongling, Qu, Siqiu
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:[Display omitted] •The MgAlCeO rare earth catalysts exhibited excellent catalytic activities.•No chemisorption O vacancies existed on catalyst surface.•The MgAlCeO rare earth catalysts obeyed a step-wise mechanism.•The effect of added water was investigated deeply. A series of well-mixed Ce-containing MgAlCe rare earth catalysts derived from layered double hydroxides were synthesized and tested for H2S selective catalytic oxidation. Particularly, no chemisorption O-vacancies but intrinsic defect sites were present on catalyst surface. Significantly, the catalysts exhibited excellent catalytic activity, reasonable durability, and outstanding sulfur selectivity (100%) at relatively low temperatures. Furthermore, the catalyst followed a step-wise mechanism, and the catalyst deactivation was due mainly to the slower oxidation rate of Ce3+ to Ce4+ by O2 as compared to the reduction rate of Ce4+ to Ce3+ by H2S. Particularly, the added water, a Lewis base, can compete with inefficient S8 catalyst for the occupation of Lewis acid sites and active sites. Meanwhile, it can change the characteristics of catalyst surface, resulting in sulfur existing form transforming from inefficient S8 catalyst to inactive S3. Thus, lead to a decrease of deposited inefficient S8 catalyst content. Consequently, decrease the catalytic activity.
ISSN:0304-3894
1873-3336
DOI:10.1016/j.jhazmat.2017.09.014